There are two reasons why this happens. The first one, which is quite obvious, is that eliminating thermal shocks, we have drastically reduced the expansion of the dies, and thus the formation of cracks. The second reason is that the alloy remains smoother, helping us fill the casting because we work at a higher temperature compared to the standard.
We have often reduced the speed of the second stage.